2700 agricultural low film unit

Digesting and absorbing advanced foreign technologies, through computer optimization design, it has the characteristics of uniform material distribution and low resistance, ensuring that film products have good thickness uniformity, shortening the time for film introduction and machine head adjustment, reducing raw material waste and consumption caused by adjusting thickness uniformity, and thus reducing the production cost of film products.

湖北省金中德科技机械设备有限责任公司

 

湖北省金中德科技机械设备有限责任公司

 

Main technical parameters of plastic film

 


Applicable raw materials: LDPE LLDPE+LDPE

Product specifications: Product width 2500mm (folded diameter)

Product thickness deviation: National standard acceptance, with a production capacity of about 3 tons within 24 hours.

 


Equipment technical parameters:

 


Single screw plastic extruder

Screw form: New type of screw with mixing section

Screw diameter: Ø 75mm

Length to diameter ratio: 30:1

Screw material: 38CrMoALA

Processing technology: quenching and tempering treatment, nitriding hardness HV ≥ 960, nitriding thickness

0.3 —0.6mm, The brittleness is not greater than level 2.

Screw material: 38CrMoALA

Processing technology: quenching and tempering treatment, nitriding hardness HV ≥ 740, nitriding thickness 0.3-0.6mm, brittleness not exceeding level 2.

Heating control: Cast aluminum heater, divided into 3 zones for heating, with a heating power of 21KW,

Double digital automatic temperature control (1.0 level temperature control meter) with precise temperature control.

Cooling control: using fan cooling, divided into 3 zones for air cooling, using centrifugal blower, with low air pressure, high air volume, and rapid and accurate temperature control.

Fan flow rate: 504 cubic meters per hour

Blower pressure: 860pa

Gearbox: Hard tooth surface gear transmission, material 20CrMoTi, quenched and tempered carburizing treatment, gear hardening treatment and surface grinding, with smooth transmission, high torque, low noise, forced circulation oil lubrication, forced water circulation cooling oil temperature, long service life and other characteristics.

Main motor: 55KW variable frequency speed regulation

Inverter: Domestic brand inverter

Extrusion rate: 180Kg/h (LDPE)

Filter screen: Adopting a new cylindrical structure, it has good sealing and no leakage,

Replacing the filter takes a long time and is convenient and quick, saving time and effort.

Cast aluminum heater, divided into 1 zone heating, with a heating power of 4.5KW

 


2、 Die head: Ф 500 die head

Digesting and absorbing advanced foreign technologies, through computer optimization design, it has the characteristics of uniform material distribution and low resistance, ensuring that film products have good thickness uniformity, shortening the time for film introduction and machine head adjustment, reducing raw material waste and consumption caused by adjusting thickness uniformity, and thus reducing the production cost of film products.

Mold head form: center feeding spiral type.

Mold material: 45 # steel, quenched and tempered treatment, hard chrome plating and polishing treatment on the surface of the flow channel, uniform chrome plating layer, high smoothness, wear-resistant and corrosion-resistant.

Gap between mouth molds: 1.8mm

Heating control: cast aluminum heater, divided into 2 zones for heating, with a heating power of 12KW

 


III Wind ring section:

Wind ring form: dam type, uniform air volume, adjustable wind direction.

Outer diameter of wind ring: Ø 1400 mm

Fan power: 7.5KW

Duct: Rubber

Stable foam system: Stable foam board

     

     

5、 Herringbone board device

Form: Grid type herringbone board

Material: Galvanized pipe

 

6、 The first traction system

Structural form: Tower type structure, detachable, with safety operating platform and safety protective railing

Center height of traction roller: 7800mm

Traction form: Roll type traction (one steel roller and one rubber roller)

Traction roller specification: Ø 175X2700mm

Material of traction rubber roller: nitrile rubber

Guide roller specification: Ø 80X2700mm

Traction motor power: 2.2KW

Traction reducer: worm gear reducer

Traction line speed: 120m/min

The sprocket is made of 45 steel and undergoes high-frequency quenching.

 


7、 Splitting device: equipped with a pair of edge profiles

 


8、 Second traction:

Traction form: Roll type traction (one steel roller and one rubber roller)

Traction roller specification: Ø 160X2700mm

Material of traction rubber roller: nitrile rubber

Traction motor power: torque motor 10N/m

Traction reducer: Cycloid pinwheel reducer

The sprocket is made of 45 steel and undergoes high-frequency quenching.

 


9、 Expansion auxiliary device: using a rotating rubber bending roller with adjustable angle

 


10、 Roll up section

Form of winding: Double surface friction winding;

Roll diameter: Ø 120X2700 mm

Linear speed: 120m/min

Winder motor: 2.2KW

Roll up reducer: worm gear reducer.

The sprocket is made of 45 steel and undergoes high-frequency quenching.

Automatic coil changing device: PLC automatic control, fixed length automatic cylinder ejection cutting, air blown film, track type moving device, automatic coil unloading.

 


11、 Electric control cabinet:

The electrical appliances are produced by the Sino foreign joint venture Delixi brand,

Counting alarm device: intelligent electronic meter reader, fixed length alarm.

 

湖北省金中德科技机械设备有限责任公司

 

 

 

url: https://hbsjzdkj.com/en/55367/376.html

Contact Us

Hubei Jinzhongde Technology Machinery Equipment Co., Ltd

Alibaba Store:hbsjzd.1688.com
Hotline:18071870860
Company Address: No. 90 Yong'an Avenue, Xian'an District, Xianning City, Hubei Province


Scan and follow us

Copyright © 2023-2043 Hubei Jinzhongde Technology Machinery Equipment Co., Ltd