Inner Mongolia Zhongke Kelan invested 500 million yuan to build a PDA project with an annual output of 33000 tons of fully natural biodegradable materials. The project is led by the incubation technology of the Chinese Academy of Sciences and aims to achieve complete degradation of soil, compost, and marine environment. It will be put into operation in two phases starting in 2025.
According to a report from the Bioplastics Research Institute, Inner Mongolia Zhongke Kelan has invested approximately 500 million yuan in the Wuhai High tech Zone Low Carbon Industrial Park to build a PDA project with an annual output of 33000 tons of all natural biodegradable materials. The project will be implemented in two phases, with the first phase producing 3000 tons per year and the second phase producing 30000 tons per year; The filing has been completed on August 1, 2025, and the planned construction period is from August 2025 to December 2029.
Founded in February 2024, Zhongke Kelan was incubated from the National Engineering Center for Engineering and Ecological Plastics, Institute of Physical and Chemical Technology, Chinese Academy of Sciences. Its founder is Dr. Ji Junhui. Its core product is the internationally leading third-generation biodegradable plastic PDA (Polymers Bio degradable in All Nature Environment), which can realize complete degradation in soil, compost, ocean and other natural environments.
On May 13, 2025, Beijing Zhongke Kelan New Material Technology Co., Ltd. announced that it had received tens of millions of yuan in angel round financing. This round of financing is led by Junke Danmu, followed by Linge Venture Capital, and Yibai Capital serves as the exclusive financial advisor. This round of funds will be used for business aspects such as production line expansion, market promotion, research and development investment, and team building.
Key Information Overview
|
Project |
Key points |
|
Main body |
Inner Mongolia Zhongke Kelan New Material Technology Co., Ltd. (relying on the Institute of Physics and Chemistry, Chinese Academy of Sciences), Wuhai Development and Reform Commission |
|
Location |
Low carbon Industrial Park, Wuhai High tech Industrial Development Zone, Inner Mongolia |
|
Scale |
Annual production of 33000 tons of PDA (Phase I 3000 tons/year, Phase II 30000 tons/year) |
|
Investment |
About 500.54 million yuan (self owned 300 million yuan, loan 200.54 million yuan) |
|
Progress |
The record has been confirmed (August 1, 2025); The pilot project has also been registered; The first phase of environmental impact assessment is in progress; The pilot base has started construction. The Development and Reform Commission of Wuhai City |
|
Time |
Planned construction start and end: August 2025 to December 2029 |
|
Technology/Application |
Fully biodegradable PDA in the natural domain, with a degradation cycle that can be customized as needed between 3 days and 10 years; Downstream oriented towards consumer electronics, marine fisheries, etc |
|
Matching |
Relying on local BDO resources and the coal chemical industry chain, promote the synchronous construction of water, electricity, and other facilities |
Project Progress and Schedule
2025-03: Signed a contract with Wuhai City to promote the pilot base.
2022-04: Complete company registration.
May 2025: Filing of pilot projects; Sign a lease agreement for the base.
June 2025: synchronized construction of element guarantee and civil engineering.
July 2025: Construction of the pilot base begins.
On August 1, 2025, the filing for the annual production of 33000 tons of PDA project was confirmed.
Alibaba Store:hbsjzd.1688.com
Hotline:18071870860
Company Address: No. 90 Yong'an Avenue, Xian'an District, Xianning City, Hubei Province
Copyright © 2023-2043 Hubei Jinzhongde Technology Machinery Equipment Co., Ltd